Index
Brand |
AI2O3 % |
Fe2O3 % |
Apparent porosity % |
Bulk density g/cm3 |
0.2Mpa Refractoriness under ℃ |
Sinterdliner change (1400℃×3h)% |
Corundum mullite brick |
<80 |
≤1.0 |
≤19 |
≥2.7 |
≥1700 |
±0.2 |
High alumina wear-resistant brick |
≥75 |
≤1.2 |
≤20 |
≥2.6 |
|
|
≥85 |
≤1.5 |
≤18 |
≥2.8 |
|
|
|
Index
Brand of name |
Refractoriness ℃ |
Abrasiveness Cc |
Crushing strength Mpa |
Bendingstrength Mpa |
Sinterdliner change (1100℃×3h)% |
Thermal stability (1100℃windcyele)次 |
Corundum mullite brick |
≥1790 |
≤6 |
≥95 |
|
|
≥40 |
High alumina wear-resistant brick |
≥1790 |
≤7 |
≥85 |
≥12 |
≤0.1 |
|
≥1790 |
≤6 |
≥100 |
≥15 |
≤0.05 |
|