Brand of name Index |
Silicon carbide castable |
Self-flow corundum castable |
High strength wear-resistant castable |
Steel fiber abrasion resistant castable |
Mullite castable |
Phosphate castable |
High alumina castable |
AI2O3 % |
≥20 |
≥90 |
≥80 |
≥70 |
|
≥75 |
≥80 |
SiC % |
≥55 |
|
|
|
|
|
≤15 |
Fe2O3 % |
|
|
≤1.5 |
|
|
|
≤1.0 |
SiO2 % |
|
|
≤10 |
|
|
|
|
Bulk density g/cm3 |
≥2.6 |
≥2.8 |
≥2.7 |
≥2.8 |
≥2.6 |
≥2.2 |
≥2.6 |
Compressive strength Mpa110 |
≥85 |
≥110 |
≥120 |
≥90 |
≥40 |
≥65 |
≥80 |
Compressive strength Mpa1100 |
≥120 |
≥130 |
≥125 |
≥100 |
≥75 |
≥80 |
≥100 |
Flexural strength Mpa110 C |
≥12 |
≥12 |
≥14 |
≥9 |
≥8 |
≥8 |
≥10 |
Flexural strength Mpa1100 C |
≥15 |
≥15 |
≥16 |
≥12 |
≥12 |
≥10 |
≥13 |
Refractoriness ℃ |
1800 |
1800 |
1800 |
1800 |
1800 |
1700 |
1800 |
The rate of change of reheating line(1100℃×3h)% |
±0.4 |
±0.1 |
±0.2 |
±0.4 |
≤-0.4 |
≤-0.5 |
±0.3 |
Thermal shock stability(1100℃windcyele) |
≥40 |
≥30 |
≥38 |
≥20 |
≥42 |
≥30 |
≥20 |
Wear resistance cc |
<5 |
<6 |
≤6 |
≤6 |
≤12 |
≤14 |
≤12 |